Thanks, Pete. I'm hoping he's back but not sure. I've been waiting to try him as I imagine the backlog of orders is nuts.

I can suggest only one other source of metal contamination in my clear. I made the Cristalica frit that I mixed with black tin by ladling into a galvanized bucket full of water. I doubt much zinc would have come off but surely some did.