View Single Post
  #20  
Old 05-31-2018, 04:12 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,713
Pete VanderLaan is on a distinguished road
I'm currently fishing about to see if anyone else is experiencing what you are seeing. It's the same as in crucibles. When I get a single call as a complaint, I always start asking around if anyone else is having the same problem. If It's "Yes", it just became my problem. If it's "No", then its another person either mistreating their pot, or just not understanding that they don't last forever.

Cullet, when it's being bad is quite indiscriminate. It goes after everyone and thy finally do compare notes. That's one of the things I love about craftweb. Strength in numbers. I have a few calls in, here and there. i'm at a loss to explain yellow. I can explain other things, but not that. Again, the stuff I have in the tractor shed is water white . I don't think the Zinc explains it at all.
__________________
Where are we going and why am I in this basket?
Reply With Quote