Staying away from this: Are you melting any cristalica without additives? What do they look like?

I have always added black tin to a raw batch, never a cullet. What I wanted was a clear that wa receptive to having such materials as Silver bromide to it and in deed it was receptive. Silver flowed on the surface, it never balled up as I would expect in an oxidized clear.