When I use anything to make Cristalica frit it has always been clear/white. The yellow color did not come on until I added black tin, melted overnight and used it the next day. I could see the tint as I gathered but it became very noticeable in the punty bucket. I haven't made frit with it after the tin addition, but I would guess it will look pale yellow.