I've always been able to glance at a tank and know somethings up before I look at the thermo readout, even if it's 50 degrees off. Know the glow.

I've gotten away with some questionable stuff at times, but I'd never make a rule of it. Or try to convince someone that it was other than a fluke. That 15% rule probably originates in the moretti crowd, you still see it posted on torch supply sites.

Watching Fero put everythig under the sun but boro on one of his birds, then put it on the table when he was done, was kind of an eyeopener. Doesn't mean I'm gonna try it.

I just saw what Glassnotes 4 was going for, putting mine in a safe.