Considering how weak the scratch from a cutter makes plate, it wouldn't surprise me if there was some significant strength loss.

I don't know which Zim it actually is, inherited a ziploc, and it strikes problem free without being buggy on its position in the production cycle. I've tried sys 96, premium 1.0, premium 2.0, and cristalica, but it spiderwebs them all.

That's kind of awful that sub par glass was the required expectation. I know when I need to get away with it, but that should never be a goal.