Stupid and Cheap? Maybe but unprepared is more like it. I am continually amazed by shops that have renters, orders, employees etc who don't even keep a backup crucible. Then, when they call, it can be three weeks to get the new pot.
Everyone gets laid off which they love, renters seek new sites, orders get cancelled.