View Single Post
  #23  
Old 12-08-2017, 05:52 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,854
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Scott Novota View Post
This is pretty cool! Where did you get those little assays from? I am interested in doing some stuff myself and those look very handy.
******
Coorstek, or you can make your own. Kyanite and ball clay
__________________
Where are we going and why am I in this basket?
Reply With Quote