I should have been clearer. Most of the time I compare colors to colors. It helps me see the effects of specific changes in the oxides used. John is quite correct about the placement of the clear if that's what you're doing.

Where I have my greatest difficulties is comparing two colors in a thick piece of work where there's no clear at all. A lot of why I prefer the ring test.