what the photo fails to show clearly is whether there is other color for the inside gather and that would indeed promote the mismatch.

The outside color appears to either have been worked really cold, so that much of the color stands proud on the surface or the color stands proud because of substantial mismatch on viscosity. Either way, it's mismatch. I very much doubt it's the annealing.

I know enough people who use commonly accessed GLASMA batches to not suspect it has some wild L.E.C. The Sys96 is a known 94.1. That going together with the GLASMA, which is in the 96-96.5 range more than enough to cause the break.

My opinion though. What do I know? I liked Jordan's answer.