Ok Pete, The torch is fixed and I have had no headache since. Of course this don't meen nothing right now cuz it's gone away for days and then returned. The deposits on the gloryhole are quite substantle and I checked the rest of them all 13 and they all have it as did our old glorys. I'll try to sneek a camera in and get a photo to show you. And as far as the lead cullet disposal is concerned, We have hoppers full of it sitting around. A truck comes in once a week and picks it up. I heard some guy uses it for something. They give it to him. When I asked about getting a half ton the answer was "Sure" There's no restrictions on cullet lead or no lead. At least not in NYS.