Additionally there is from Zicar

MICROSIL Microporous Insulation

Max Use Temp 1742F

68F .132
392F .145
752F .173
1112F .208
1472F .263


Alumina Mat

Max Use Temp 3002F

315F .50
1000F .77
1400F 1.03
1796F 1.33
2192F 1.65
2597F 2.15


Alumina Blanket Type AB & MB

Max Use Temp 2912F

599F .50
1000F .70
1400F .90
1796F 1.25
2192F 1.60
2597F 2.15


Alumina-Silica Blanket Type ASB-2300 & ASB-2600

Max Use Temp 2300F and 2600F

Bulk Density of 4 pcf

500F .56
1000F 1.13
1500F 1.96

Bulk Density of 6 pcf

500F .45
1000F .94
1500F 1.70
2000F 2.80

Bulk Density of 8 pcf

500F .39
1000F .78
1500F 1.31
2000F 2.02

Bulk Density of 10 pcf

1000F .73
1500F 1.17
2000F 1.72


Alumina Insulation Type ZAL-15 & ZAL-15AA board

Max Continuous use 2822F & 2732F

482F .40
977F .60
1472F .90
1967F 1.30
2282F 1.70
2462F 1.80


Alumina-Silica Insulation Type AXL Board

Max Continous Use 2300F

752F .80
1472F 1.20
2012F 1.50


Alumina-Silica Insulation Type AXHTM Board

Max Continous Use 2600F

752F .60
1472F 1.00
2012F 1.70


There are a few more if anyone is interested.

ed