That well may be true but if it is the case, it strikes me that the big sales pitch regarding the sys96 colors would be drop dead easy to match to the clear. That was the point.

If what you say is true, and the two are different, is it the case that the colors matched both glasses? One was measured at a 94.1, the other as you suggest is a true 96.

They should not fit each other if that is true. I do view .5 as a lot.