I have no doubt that the way the nuggets are treated is remarkably different, or that the formula is tweaked from the base clear, I've melted the flat scraps. Just doesn't explain why system "96" sheet glass would be compatible with system "96" base cullet, with it's measured coe of 94, and not also be 94. If the sheet is a true 96, then why is it compatible with a 94, but not all the other 96 out there?