Originally Posted by Art Freas View Post
I always here the 94.1 number from tests done before the "improved System 96 Studio Nuggets" I am really curious to see if the improved low/no borax formula is still 94.1. My understanding is that Oceanside is producing that one. I am also curious to see if the Oceanside version is the same from an expansion perspective as the "Improved System 96 Studio Nuggets"
*****
You can do a simple measurement your self doing a simple pull test between the two clears. Heat them both up in the box and make balls of each , weld them evenly and pull them out straight. If you get a straight cane, they have similar expansions. Once you have looked at it, anneal the cane and look again.
__________________
Where are we going and why am I in this basket?