Originally Posted by Franklin Sankar View Post
Eben by cold you mean after you maver and form a skin? And the inside still hot? If the glass get too cold why donít you give it a little reheat. Can reheat replace your blow and cap step?

Franklin
Yeah mon. Cold skin. Hot core