In fact I just checked on your spreadsheet and the silicon % of my mix is 64.94%. I don't know what I did wrong with my division and what I thought was more like a 55.4% sand content. Maybe I'm just calculating weight percentage and not thinking hard enough about oxide percentages which the spreadsheet seems to be accounting for?