By the way, lead cullet is a hazardous waste and has special (as in EPA mandated) disposal requirements. Lenoux used to pay $600.00 a ton to send their cullet to a recyler that processed it to remove the lead. There is a way to melt electrically that causes the lead to return to it's elemental form. (I don't exactly how it works, just that it does)