These are actual dimensions taken from the 200# castings.

The center support piece in the tub is a 3x2x1/4 sq.tube w/ 2x2x3/16 angle fitted.
scrap pieces of stretched metal make up the flooring.
The tub is 12”x ¼ x 44”dia.<(200#)
three casters n brackets welded permanently.

As far as insulating the bottom end, I’ll be using a layer of tin foil, 5 layers of 1900 insblock fiber board, one course of 2300 brick layed flat, plus the 4” of casting….

__________________________________________________ ____
I’m needing a 50 kva single phase transformer…so far ebay hasn’t worked out so good...can you help?