This might sound stupid, but to be honest I have no clue.


Pete when your are adding stuff to cullet, do you melt the cullet down then add to the melt and mix? Do you mix it all up and add it to a cool pot and bring it up and mix? What about batch is it the same process?

I have never melted anything besides clear so I have no clue what the process is and have a missing bit of information at the start.

I don't plan to make color without taking a class but I do hunger for the knowledge of the process.