no less than 2300F. Screen it well. Small charges. Proof after each charge and hold the charges until the proofs show no unmelted stuff. The path to phosphate opals leads to madness.
You are not going to like this stuff for murrinis. It is not dense enough. Incredibly beautiful as a stand alone. The viscosity will be very similar to your basic clear.
|