Thread: Phosphate Opal
View Single Post
  #19  
Old 12-06-2006, 06:30 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,265
Pete VanderLaan is on a distinguished road
when I try to make it better, lots of times I just make it different. We call it another triumph of hope over experience Pay attention to lowering the phosphate content as John Suggests. 4% is nice.
Reply With Quote