For the wire furnaces...
View Single Post
#
35
03-21-2004, 02:23 PM
Brian Gingras
Guest
Posts: n/a
Re: Rule of Thumb
Quote:
Originally posted by F Thumb
1/10th of an amp per pound of glass. Works for me.
wouldn't a figure based on Watts per pound be more accurate, as 20 amps at 120v is not the same as 240 or 208?