There comes a point where describing melting energy in pounds becomes pretty non-descriptive.
A 200lb pot is almost the same size as a 300lb pot, same for 80 and 100.
What always makes the difference is the size of the furnace itself, watts per cubic foot will probably be the best standard.
|