My minimal experience with ultra thin tests is that the gaps are far more exaggerated then they are on a thicker one. My tests are usually around 1/4- 3/8ths inch thick total. I put them in a zip lok with notes when I've done the scoring.

I don't care for the test they use at either bullseye or Uroboros. I would at that point prefer a Hagy seal. It tells you a lot more.