Given the complete color range they choose to use with varing levels of mismatch, I suspect hot pops would very possibly become a breakage issue. My work with them allows for easy breaks if the color is monolithic but not so much with other glasses. They would still need a flame polish or belt work after that regardless. Then you have to reanneal. \

Popping off is not quite as simple as it sounds.
Firing workers if true, is a real issue.