I think GLASMA is a beautiful glass. I think it requires operator experience to melt it or it does form tiny stones melted too hot. That at least has been my experience and I've been at it for a while. Price is sorta kinda an issue but I tend to think all batch prices to be in flux right now. I continue to expect to see the sole supplier cullet to go up substantially. Spruce Pine continues to be the least expensive alternative on the market today. I continue to make my own glasses as I have for almost fifty years.

Also Sam, I think you meant undeserved, not underserved but I could be wrong.
__________________
Where are we going and why am I in this basket?