I have similar advice as Jordan. I would clamp them in a vise at the pivot point and gently tap them in. Rinse repeat. Do not grind or file the mating surfaces that is the one thing that makes repair almost impossible. If they are not flat at the mating surfaces you can lay them on the anvil or flat anvil like object with the flat surface towards the anvil several taps should lay them flat to the anvil.

It is really hard to understand the problem so any advice without seeing what the problem is could do more harm then good. Do not hammer on the mating surface of the shear.