Given that charge cycle, the pot should last quite a long while. It seems quite cold to me. I'm charging now and pretty much run it up to 2250F before I start. Keep in mind that all of these issues undergo quite a change when there's no flue and that is the case with most wire melters which in turn makes the glass formation a real issue.