I usually use a modified from of suppio... it works well for transparent colors, and thicker cane made with duro. Basically make a dense overlay, or thick cane roll up, gather over once, and make a tube about 18"-20" long. Once annealed, saw into 2"-2.5" sections, then wash, then bring up in the pick up box, stab it up on a collar, and then use as you normally would.