View Single Post
  #35  
Old 03-30-2005, 12:26 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,681
Pete VanderLaan is on a distinguished road
Quote:
Originally posted by Robert Mickelsen
I know the green was tested on a dilatometer and was on the money. The color manufacturers have tried for years to solve the problem to no avail. You are absolutely correct in what you say about the present group of suppliers.
***************************
Is this that green that was a square stick and came from the phillips plant in NY along with the opaque white stick about three years back? Secondly , who did the dilatometry tests? Do you really know firsthand that it was tested? That's what I mean about the suppliers.
Reply With Quote