Based on the work Durk did on microgram release per hr in the tank or pot as directly related to furnace temps, I can't see that occurring. One has to wonder why Fero is so secretive about even admitting what they melt in this country. Hammond got out of the lead monosilicate biz here a few years back although Hammond Lead of Shanghai sells it readily.

It's my impression that Cadmium is far more difficult to filter than any of the other metals in its entirety. It is not difficult to ruin a torit filter and they are expensive. Scott, did they make mention of Selenium as well? That's pretty volatile stuff as well.

This event is why Mark went to Italy with a non toxic ultra dense white for filigrana but there are issues.