The rails the door is on are adjustable. As the door slides to the left it swings out by about 15 mm. When it closes it only leaves about 2 or 3 mm clearance. I might not have experience in blowing but not bad in fabricating. The glory actually reached 2260 in half an hour. And then reduced the propane as I thought it was enough for a test run. I will try it again tomorrow and see how high it will reach before I put the fibre sheeting.