Originally Posted by Shawn Everette View Post
Trade name, it's just vermiculite board. It's supposed to tool nicely and be fine at the temps I'm wanting, that's why I'm interested. Also minimal on the dust end of things.
I've been using 1" vermiculite board as the roof of my annealer for about a year now. The rest is brick. It's been great so far. Backed by 2" of frax. No sag or breaking down that I can see.