Thread: Color bubbles
View Single Post
  #30  
Old 11-03-2017, 10:46 AM
Kenny Pieper Kenny Pieper is offline
Registered User
 
Join Date: Feb 2003
Location: Burnsville N.C.
Posts: 867
Kenny Pieper is on a distinguished road
Quote:
Originally Posted by Scott Benefield View Post

Lino's rosin black was all that, but the melts he was doing at the old Manifesto facility were kind of unpredictable. Very fine bubbles would only appear in the final application, but not in the initial cane pull--occasionally. It was impossible to know if you had a good melt until you had taken it that far, but by then you were stuck with whatever you had. Lots of it went into the landfill.
I have melted that black a couple of times with no problems. Its crazy how it catches on fire when it gets charged. I stays black that's for sure!
Reply With Quote