Quote:
Originally Posted by Sam Stang View Post
Any batch requires operator experience, Peter. I happen to think that Glasma is easier to deal with than Spruce. And it melts at a much lower temperature which translates to energy savings and significantly longer furnace/crucible life. I don't like the fact that it is shipped from overseas. I wish there was an equivalent, locally made product.
Doesn’t it take you 2 days to fill your pot though?