Quote:
Originally posted by Pete VanderLaan
John and I both made the color first, and then adjusted the glass to a 96.
|
Pete, I’d still argue that you weren’t adjusting to a 96 COE, you were adjusting to fit SP87.
Do all glasses with a 96 COE fit SP87?
And you think viscosity is confusing?
BTW what’s the AP of SP87?
Quote:
Originally posted by Pete VanderLaan
Why did lead seemingly defeat the compatibility problem up until you pierced the surface tension of the piece with a saw or a grinder?
|
I don’t understand how the compatibility problem is even “seemingly” defeated if it’s only compatible until you cut into it.