I can only assume that youi think I still buy my Black Tin from Goldschmidts since that was my last known reference when I still was allowed to post at Handmade. I gave up on them a long time ago. Nice stuff but too much at a time and too pricey.

The interesting thing I am doing right now with the cad sel red is making five inch diameter logs from it about 16 inches tall. When cooled, I cut them up ( I'm practising for logging in New Hampshire) and make them into 3/4 inch thick rectangles and then polish them. The color is not to be believed! I will use them in some solid optics pieces I am going to start in May. Copper reds can't compare and I was hooked on copper ruby for thirty five years. This is mo bettah.