This is Christian Thorntan's mix that he uses for his factory down in Mexico. It raises the expansion of container glass to let it work with the commercial color out there and maybe softens up the glass a bit to help the workability. Last I heard he was selling it to people who want to do a similar thing. It's probably not a tough thing to figure out on your own if one was interested. It's not rocket science people.

He was scheduled to give a talk at the San Jose GAS conference but wasn't able to make it but one of engineers came and gave an excellent presentation on what they are doing on the energy efficiency front. I would have to say from the looks of it he's probably doing more with that kind of thing than anyone else right now.