That density is probably correct. In the STP melts I've done, it is periodically really streaky stuff, almost like a comb was run thru it but if reannealed, it really took on opacity. Press molding will no doubt do something unexpected but the re strikes matter a lot. Streaking seems to be a repeat concern with it. Kenny wrote me about that last week and I really didn't have great insight. Keep the calcium as low as humanly possible.