AP

You mention AP, great but at Log 13.4 ?
At Leerdam the batch calc program spitted out Log 2 down to 7 and Log 13.4 as AP
Philips mentions Log 12.4 Pa.s as AP and 13.5 as SP. The area in between is regarded annealing range in their info.
GLASMA through Glafo talks about transformation temperature at Log 13 in Pa.s
So what's the consensus here?