So on my Stadel mini I found three lairs of fairly dense fiber about 1 inch thick against the casting and that was backed with less dense frax out to the metal shell.In fact there was a bunch of ''chop'' next to the shell

What's the 1 inch stuff?

If I replace the 3 one inch lairs with some dense 3'' frax and another 3 inches of the same weight, is that going to make a difference in the heat loss?