Ok single induviduals, Im talking about the bigger picture, making it possible for small studios to have a palate of hundreds of colors, no one person can do that. Of course the knowkedge is at Corning or the institute , but not one person can accuire that for the glass.yes you can melt a color or two,but its not possible for the small studio to melt hundreds of colors.
My experience is that everyone was very secretive 30 years ago