Quote:
Originally Posted by Lawrence Duckworth View Post
Steve S. recommended a 15kva 240 input, 45v output single phase transformer with standard 5% and 10% voltage compensation taps.

Do you guys plug the cleanout with brick and fiber?
***********************
And while that is absolutely the best unit for the job, you aren't going to find it off the shelf. It's a custom transformer.
__________________
Where are we going and why am I in this basket?