Brian, thanks so much for your help. I’ve been down there a couple times now and sure wish I would’ve bumped into you…

I’m getting close to tackling the door and s/s front. The expansion is something to ponder for sure…and the weight of the door too, maybe a counter weight on the backside of the bridge assembly.

The skin is 26 ga.coil stock from the local metal roofing supply house, probably should have gone with something heavier, (16ga.nmaybe??) anyway, fastened with a strap and 2- ¼-20x5/8” ea. I’m guessing the skin is in four sections for expansion, otherwise a sheet of stainless would have been a bunch quicker and less hassle…but then wrenching all the nuts down kept my middle granddaughter busy.