Thanks Art, I do have a wifi cam pointed at both of my furnace controllers, which are super handy and I wouldn't want to run without them now, but they don't give me the alerts when needed. My backwoods DSL is occasionally spotty, and even though I get notifications that the camera is off when there's an issue, it mostly isn't the case for me that my safety system has tripped when that happens, usually just an interruption in the internet signal.