It includes a senermont analyzer but no other attachments. I can't see any obvious need for others but I would not want to be without this attachment.
Testing is such a strange pursuit. I don't really think all that many studios even have decent sized diamond saws and that makes ring testing hard. Clearly, dilatometers are close to non existent. I don't sense much interest in testing anyways. The number of people making color is small. I think the real mismatch problem is really with the cullets available and in my mind that should simply not be happening, but it is. Making your glass a 96 is not hard.