Quote:
Originally Posted by Jordan Kube View Post
A custom clear with an offset expansion would be the way to go. This doesn't work with batch.

This is after 24 hours in the pot. Again, the pictures don't capture how nice this stuff is. It was the only one I could get out today, the barlett controller decided it didn't want to clear its error message so things are coming down as we speak.
Is that straight out of the pot , or did you have to strike it? Nice color!