Cristallica would be making a huge mistake not learning from the Spectrum debacle. After 3 years of running the Spectrum with borax through 1000# Wetdog furnaces they were trashed. After 2 years running the no borax formula they look like they could definitely beat that by a year or two. Nobody should have to put up with the glass destroying their furnace. It was total bullshit that Spectrum let it go on so long.