Quote:
Originally Posted by Art Freas View Post
We are working with the Cristalica and initially we tried 2100 but it was just too thick to get the gathers we wanted. It was hard to get the right amount to work thin without taking a lot off the pipe. We now work at 2125.
****
That's what I meant when I said you tool up for what you are making. Efficiency keeps you from being exhausted. Sometimes you can turn it down, sometimes up. That's far more flexible than most tooling in the shop.